dc.contributor.author Park, Jeong Hwa -
dc.contributor.author Im, Ha-Ni -
dc.contributor.author Lee, Kang Taek -
dc.date.accessioned 2021-10-17T02:30:09Z -
dc.date.available 2021-10-17T02:30:09Z -
dc.date.created 2021-09-17 -
dc.date.issued 2021-09 -
dc.identifier.issn 1229-7801 -
dc.identifier.uri http://hdl.handle.net/20.500.11750/15544 -
dc.description.abstract Abstract: Solid oxide fuel cells (SOFCs) are promising energy conversion devices because of their high electrical efficiency, even for small power systems. However, when the anode is exposed to reduction and oxidation (redox) cycles, the Ni phase causes a large microstructural change as a result of its chemical expansion and contraction. This negatively affects the electrochemical performance. However, most studies have focused on the redox cycling behaviors of SOFCs at high operation temperatures (≥ 800 °C). Therefore, in this study, we investigate the degradation behavior of the SOFC anode during redox cycles at 500 °C. To identify the individual steps of the electrochemical processes of the anode, in-situ monitored impedance spectra were analyzed using the distribution of relaxation time method at various oxygen and hydrogen partial pressures. Consequently, the electrode polarization process was deconvoluted into five sub-processes. During the redox cycles, three major peaks were altered: gas phase diffusion in the anode substrate (10–1–101 Hz), gas diffusion coupled with charge transfer reaction and ionic transport (102–103 Hz) and charged species across the Ni–yttria stabilized zirconia interface at the anode (103–104 Hz). The major degradation of the electrode performance at 500 °C was attributed to the increase in gas phase diffusion resistance due to Ni phase aggregation and the decrease in porosity in the anode during the redox cycles. This was confirmed by microstructural analysis. By contrast, the other two processes (102–103 and 103–104 Hz) compensated each other, thus having negligible effect on performance degradation. Graphic abstract: [Figure not available: see fulltext.]. © 2021, The Korean Ceramic Society. -
dc.language English -
dc.publisher Springer -
dc.title Understanding redox cycling behavior of Ni-YSZ anodes at 500 degrees C in solid oxide fuel cells by electrochemical impedance analysis -
dc.type Article -
dc.identifier.doi 10.1007/s43207-021-00136-2 -
dc.identifier.wosid 000688362200001 -
dc.identifier.scopusid 2-s2.0-85113376412 -
dc.identifier.bibliographicCitation Journal of the Korean Ceramic Society, v.58, no.5, pp.606 - 613 -
dc.identifier.kciid ART002761471 -
dc.description.isOpenAccess TRUE -
dc.subject.keywordAuthor Electrochemical impedance spectroscopy -
dc.subject.keywordAuthor Distribution of relaxation time analysis -
dc.subject.keywordAuthor Solid oxide fuel cell -
dc.subject.keywordAuthor Ni-YSZ anode -
dc.subject.keywordPlus DEGRADATION -
dc.subject.keywordPlus TEMPERATURE -
dc.subject.keywordPlus ELECTROLYTES -
dc.subject.keywordPlus PERFORMANCE -
dc.subject.keywordPlus MECHANISMS -
dc.subject.keywordPlus CATHODES -
dc.subject.keywordPlus SPECTRA -
dc.citation.endPage 613 -
dc.citation.number 5 -
dc.citation.startPage 606 -
dc.citation.title Journal of the Korean Ceramic Society -
dc.citation.volume 58 -
dc.description.journalRegisteredClass scie -
dc.description.journalRegisteredClass scopus -
dc.description.journalRegisteredClass kci -
dc.relation.journalResearchArea Materials Science -
dc.relation.journalWebOfScienceCategory Materials Science, Ceramics -
dc.type.docType Article -
Files in This Item:

There are no files associated with this item.

Appears in Collections:
ETC 1. Journal Articles

qrcode

  • twitter
  • facebook
  • mendeley

Items in Repository are protected by copyright, with all rights reserved, unless otherwise indicated.

BROWSE